Kaxite Sealing manufactures the KXT-1020 flat metal foil reinforced graphite gasket at our Ningbo plant, for the flanges where a tanged metal core would leave marks on the flange face. A solid flat metal foil insert sits between two expanded graphite sealing layers, giving the gasket the same 200 bar pressure rating as the tanged variant while keeping both sealing faces perfectly smooth. The result: high-pressure performance against soft, freshly machined, or non-metallic flange faces — without scoring the surface that it has to seal against.
The flat foil core is bonded between two expanded graphite sealing layers. Unlike the tanged metal version, both graphite faces stay smooth — so the gasket seals against soft or freshly machined flange faces without leaving scratch marks, while still carrying 200 bar.
| Property | Value | Standard / Note |
|---|---|---|
| Model | KXT-1020 | Kaxite flat metal foil reinforced graphite gasket |
| Construction | Solid flat metal foil insert bonded between two expanded graphite sealing faces | Adhesive-bonded composite |
| Density | 1.0 g/cm³ | Sheet density |
| Compressibility | 15 – 35 % | ASTM F36A |
| Recovery | ≥ 20 % | ASTM F36A |
| Pressure Rating | 200 bar | Design pressure at the flange |
| Temperature Range | −240 °C to +550 °C | Same full range as the graphite family |
| pH Range | 0 – 14 | Full acid to alkaline service |
| Faces | Smooth on both sealing faces | Flat foil core — no tanged perforations |
| Eyelets | Available with or without | Optional bolt-hole protection |
| Dimension Standard | ASME B16.21 / DIN 2690 | Custom sizes to drawing on request |
| Certification | UL certified | Certificate reference available on request |
The flat foil gasket is a three-layer composite. The graphite sealing layers perform the actual seal; the solid foil core does the mechanical work — resisting blow-out, resisting crushing under bolt load, and holding the gasket in shape during handling and fitting.
Smooth expanded graphite surface against the flange. Provides the temperature, chemical and sealing performance the gasket is specified for.
Continuous metal foil, not perforated and not tanged. Provides blow-out resistance and crushing resistance, and keeps both outer faces flat rather than raked.
Second smooth expanded graphite surface against the mating flange. Both faces seal; the metal core never touches the medium.
For flanges that need more handling rigidity than a flat foil core can provide, the Graphite Gasket Reinforced with Metal Mesh Insertion is the version to consider. For high-pressure flanges without a delicate face, the Tanged Metal Reinforced Graphite Gasket is normally more economical.
All four gaskets in the Kaxite graphite family use the same expanded graphite sealing material and cover the same −240 °C to +550 °C and pH 0–14 range. The reinforcement is what changes — and the reinforcement should match the flange, not the other way round.
Core: solid flat metal foil between two smooth graphite faces.
Pressure: 200 bar. Faces: smooth both sides.
Best for: heat exchanger and valve bonnet flanges where the machined face must stay scratch-free, plus soft or non-metallic faces under high pressure.
Core: perforated tanged metal, graphite locked into the perforations.
Pressure: 200 bar. Faces: standard graphite finish.
Best for: high-pressure flanges with hardened steel faces and pressure spikes, where maximum blow-out resistance is the priority.
Core: wire mesh insert.
Pressure: highest in the family. Faces: standard graphite finish.
Best for: large-diameter vessel flanges and manway covers where handling rigidity matters more than face finish.
Core: none — 100% expanded graphite.
Pressure: 40 bar. Faces: pure graphite on both sides.
Best for: non-standard shapes at the chemical or temperature extreme, where the 40 bar pressure limit is acceptable.
Confirm ASME B16.21 or DIN 2690, nominal size, pressure class, thickness, eyelet requirement and — importantly for this model — the flange face material and finish. Face condition decides whether flat foil is the right core.
For standard ASME and DIN sizes, no drawing is needed. For non-standard flange shapes, oval handholes, rectangular access covers and manifold gaskets, send a DXF, PDF or physical sample and our engineers confirm the bolt circle, gasket OD and eyelet positions before cutting starts.
Die cut or CNC cut to the confirmed dimensions. Eyelets are then fitted if they were ordered. The flat foil core is checked for continuity after cutting — a damaged foil core is a rejected gasket, because the core is what provides the blow-out resistance.
Dimensional check against the ordered standard. Material certificate, ASTM F36A test report and UL certificate reference available on request. Gaskets packed flat between rigid boards to protect the smooth graphite sealing faces during transport.
The KXT-1020 is a three-layer composite: expanded graphite on both faces with a solid flat metal foil insert between them. The graphite provides the temperature, chemical and sealing performance; the flat foil core provides blow-out resistance and crushing resistance under high bolt load. Unlike the tanged metal version, both graphite faces stay smooth — so the gasket seals against soft, freshly machined or non-metallic flange faces without leaving scratch marks.
Both carry the same 200 bar pressure rating and the same temperature and pH range, so pressure is not what separates them. The choice is made by the flange face. On a hardened steel face, the tanged metal KXT-1010 is more economical and handles pressure spikes well. On a soft, machined, non-metallic or glass-lined face — or any flange where the surface finish must stay scratch-free — the flat foil KXT-1020 is the correct choice.
Yes, in pressure rating: both are rated 200 bar with recovery ≥20% and compressibility 15–35% to ASTM F36A. The difference is where the mechanical strength is concentrated. The tanged version locks the graphite into perforations, giving slightly higher blow-out resistance under severe pressure spikes. The flat foil version bonds the foil continuously, giving a smoother face. For most heat exchanger and valve bonnet service, the flat foil is more than strong enough and the smooth face is the more valuable property.
Eyelets are metal rings fitted into the bolt holes to protect the graphite from bolt-head crushing and to improve handling. They are optional — the gasket seals without them. Eyelets are commonly specified on high-pressure flanges and on gaskets that will be reused after inspection, and they are available on the KXT-1020 on request.
Material certificate and dimensional report against the ordered standard are available per shipment on request. ASTM F36A test report — including compressibility and recovery — can be supplied for critical service. UL certificate reference is available on request. Gaskets are packed flat between rigid boards to protect the smooth sealing faces.
Standard ASME and DIN sizes ship from stock sheet. Custom-cut shapes, eyelet versions and split gaskets are produced to order. For the MOQ and lead time on your specific size, send the standard, nominal size, thickness, eyelet requirement and quantity through the inquiry form — our engineers reply within one business day with pricing and delivery.
Include the gasket standard (ASME B16.21 or DIN 2690) or a drawing, the nominal size and pressure class, the thickness, the flange face material, and the quantity. Our engineers reply within one business day with pricing, type confirmation and lead time — and will flag if flat foil is not the right core for your face.